9# Xing Yuan Rd. Haihe Industrial Park, Jinnan District, Tianjin city China—300350
+86 - 022 - 88518898, 86-477-4688189
Larger photo of cored wire (finished products)
Modification of inclusions by combing with oxide inclusions
and making it liquid at steel making temperatures, thereby
avoiding nozzle clogging in continuous casting. Improving
isotropic properties of steel. For Deoxidation along with
modification of inclusions. For low silicon grade steels.
2830% Ca, 5862% Si
30% Ca, 70% Fe
CaAlFe
30% Ca, 25%Al BalFe,
Calcium Aluminum Alloy
CaAl 75% [(Ca75%Al25%) or
(Ca60%Al40%)]; Fe25%
Lead (Pb)
99% Pb Min.
For improving mach inability of steel
Sulphur (S)
99% S Min.
For Resulphurising and improving mach inability of steel
Carbon (C)
98% C Min.
For Recarburisation of steel
Tellurium (Te)
6570% Te, 30% Mn
For improving mach inability of alloy steels
Al Cored Wire (Al)
98% Al
For effective Deoxidation with higher efficiency
than solid wire. Wire diameters upto 25 mm for large vessels
Ferro Titanium (FeTi)
70% Ti, Bal Fe
3540% Ti , Bal Fe
Deoxidation and Degasification of steel stabilization
of carbon or nitrogen. Increases formabilit
Ferro Boron (FeB)
1820% B, Bal Fe
Increases harden ability of steel. Even 0.0010.003% B can retain some of the secondary
hardening elements in alloy steels
Ferro Niobium (FeNb)
6065% Nb, Bal Fe
Improves cold ductility. Improves grain refinement.
Ferro Vanadium (FeV)
5055% V, 1% Al Max
Alloying addition for secondary hardening in alloy steels.
FerroSilicon Zirconium (FeSiZr)
3035% Zr, 55%Si, BalFe
Increases wear resistance, decreases the adverse